Black oxide coating and its effectiveness on prevention of hydrogen…
www.phase-trans.msm.cam.ac.uk/2018/black_oxide.pdf16 Oct 2018: Figure 13. (a) Bright field TEM image of the magnetite and steel substrate interface. ... The obtained selected-area diffractionfrom regions ( SA1–SA3) could be indexed as Fe3O4confirming the oxide layer is crystalline magnetite.