Hydrogen_revised6
www.phase-trans.msm.cam.ac.uk/2014/Han.pdf29 Mar 2014: outcomes of typical tensile tests. The purpose of the present work was, therefore, to study. ... charged alloys and their macroscopic uniaxial tensile test curves with respect to the hydrogen. -
Degradation of nanostructured bainitic steel under rolling contact…
www.phase-trans.msm.cam.ac.uk/2014/SB_RCF.pdf18 Sep 2014: The fatigue resistance in a varietyof uniaxial tests has been proven to be excellent [11, 14, 16]. ... All tests were performed at a rotational speed of3600 rpm (the design of the test rig allows 2.4 stress cycles per revolution)and a Hertzian pressure -
About Calculating the Characteristics of the Martensite-Austenite…
www.phase-trans.msm.cam.ac.uk/2014/MA_Bhadeshia_2013_TMS.pdf30 Jan 2014: the test specimen samples a brittle zone then the recorded value of toughness is small [3]. ... in the test used to determine toughness? 3. Does the shape of the LBZ matter? -
AuthorInstructions2.dvi
www.phase-trans.msm.cam.ac.uk/2014/LBZ.pdf25 May 2014: They usually contain untempered martensite that can lead toscatter in toughness data when the test specimen samples a brittle zone [2]. ... 3. Does the shape of the LBZ matter? 4. How many tests are required in order to establish a probability of failure -
paperbainiterollingsliding.dvi
www.phase-trans.msm.cam.ac.uk/2014/rolling_sliding.pdf21 May 2014: 9]. All the data are from tests with similarconditions of rolling/sliding. 7. ... 3.7. X-ray diffraction. X-ray diffraction spectra taken before and after wear tests are illustrated in Fig. -
al_effect.dvi
www.phase-trans.msm.cam.ac.uk/2014/al_effect.pdf13 Jul 2014: parameters. Tables 1 and 2 showthe convergency test results with varying ENCUT and k-points, respectively.Thus, it was found that Al reduces the hydrogen solution energy. ... Table 2Convergence tests results of the energy per atom in bulk Fe32, Eatom(Fe32 -
Austenite in transformation-induced plasticity steelsubjected to…
www.phase-trans.msm.cam.ac.uk/2014/multiple.pdf23 Jul 2014: Interrupted tensile tests wereused to assess the stability of austenite, and the austenite fraction in theuniformly strained region was measured using X-ray diffraction. ... 3.2. Mechanical properties. Figure 8 shows the tensile test results for alloys A -
White-etching matter in bearing steelPart 2: Distinguishing cause and …
www.phase-trans.msm.cam.ac.uk/2014/cause_Solano_MMTA_2014.pdf30 Aug 2014: The tapered loading cups were changedevery four tests and turbine oil BP2380 was used as a lubricant at room. ... All tests were performed at a rotational speed of3600 rpm (the design of the test rig allows 2.4 stress cycles per revolution)and a Hertzian -
Effect of tempering upon the tensile properties of a novel bainitic…
www.phase-trans.msm.cam.ac.uk/2014/Tempering.pptx31 Aug 2014: Linear hardening from the yield point to fracture. The elongation is higher after tempering, also the toughness as measured by energy consumed during tensile test (area under tensile curve). -
Thesis for Doctor of Philosophy Application of Lower Bainite ...
www.phase-trans.msm.cam.ac.uk/2014/Thesis_ChaeJY.pdf6 Dec 2014: The. fatigue test measures number of cycles to failure by the stress cycling. ... tests for some 109 cycles would take about a year, whereas ultrasonic fatigue test.
Search history
Recently clicked results
Recently clicked results
Your click history is empty.
Recent searches
- `Scholarship in the allocation` (7) · moments ago
Recent searches
Your search history is empty.