search results for KaKaoTalk:ZA31 24 24 |u:www.phase-trans.msm.cam.ac.uk
where 0
match all words and 19
match some words.
Results that match 2 of 3 words
-
paper.dvi
www.phase-trans.msm.cam.ac.uk/2013/Multiple.pdf20 Jun 2013: Of the 24 possibleorientations of martensite that can form in any given grain of austenite, some will be favoured andothers opposed since they do not comply with the stress - in other ... Therefore, the sign and magnitude of themechanical driving force -
ICASS
www.phase-trans.msm.cam.ac.uk/2006/ICASS.pdf26 Mar 2013: The 3rd International Conference on Advanced Structural SteelsGyeongju, Korea, August 22–24, 2006,. ... 0.83 1.57 1.98 0.24 1.02 1.54 [15]0.78 1.49 1.95 0.24 0.97 1.60 0.99 [15]. -
Microsoft PowerPoint - 130523_GIFT_Seminar_Tsuzaki(pdf) [互換モード]
www.phase-trans.msm.cam.ac.uk/2013/Tsuzaki.pdf28 May 2013: Materials Research for Environment and Energy. - 11 -. Moreover, stress corrosion cracking [19] and hydrogen embrittlement [20-24] are observed. ... Zhao, J. Sietsma, Proceedings of HMnS (2011) CD-ROM.[24] M. Koyama, E. -
Computational Design of Advanced Steels H. K. D. H. ...
www.phase-trans.msm.cam.ac.uk/2013/Genome.pdf27 Oct 2013: It has been known in this contextthat bainitic ferrite is supersaturated with an excess of carbon [24–27]. ... The accumulated evidence indicatesthat the excess carbon in the ferrite is reluctant to partition into the resid-ual austenite [24,29–33]. -
Interphase precipitation in Ti–Nb and Ti–Nb–Mo bearing steel J. ...
www.phase-trans.msm.cam.ac.uk/2013/interphase_Jang_MST_2013.pdf22 Feb 2013: Two prolonged aging treatments wereadditionally conducted to investigate the coarsening ofcarbides, where the specimens were encapsulated inevacuated quartz tubes and held for 24 and 120 h at650 and 700uC respectively. ... Corresponding author, email -
Multiple, simultaneous, martensitic transformations Implications on…
www.phase-trans.msm.cam.ac.uk/2013/multiple_martensite.pptx21 Jun 2013: 10. 11. Kinetics of martensite. Koistinen and Marburger (1959). 12. Each of 24 variants in a given austenite grain will have a different martensite-start temperature. -
Austenite stability and heterogeneousdeformation in fine-grained…
www.phase-trans.msm.cam.ac.uk/2013/bands.pdf12 May 2013: The grain size of the sample studied is extremely fine, andfine grains are associated with a reduced ability to work hardnen [24]. ... 24] A. A. Howe: Materials Science and Technology 16 (2000) 1264–1266.[25] J. -
surface.dvi
www.phase-trans.msm.cam.ac.uk/2013/surface.pdf9 Oct 2013: 24] J Krueger, HD Kunze, E Schuermann, E Fromm, E Gebhardt, Gas and carbonin metals, Springer-Verlag, Berlin, 518–613, 1976. ... phase single H atom 0 layer 1 layer 3 layers. ferrite 0.19 0.24 0.20 0.19. -
Austenite Grain Growthin a Nuclear Pressure Vessel Steel H. ...
www.phase-trans.msm.cam.ac.uk/2013/AGG.pdf2 Feb 2013: Ni. [18]. Low. C-M. n”. 24.27. 10. 12. 278.8. [24]. Low. ... Acta Materialia,. 19(4):279–286, 2006. [24] S. Nanba, M. Kitamura, M. Shimada, M. -
paper.dvi
www.phase-trans.msm.cam.ac.uk/2013/Cottrell_2013.pdf19 Oct 2013: Kozeschnik, H. K. D. H. Bhadeshia, Materials Science and Technology 24 (2008) 343–347.[16] M. ... London, U.K., 1988, pp. 309–314.[24] M. Peet, S. S. Babu, M. -
Effect of retained austenite and high temperature Lavesphase on ...
www.phase-trans.msm.cam.ac.uk/2013/maraging_Ooi_MSEA_2013.pdf4 Jan 2013: fracture [24, 25]. An experiment was conducted in which the tensile test was video recorded. ... 24. 2 Effect of heat–treatments on the measured retained austeniteaustenite content and mechanical properties. -
coarsening.dvi
www.phase-trans.msm.cam.ac.uk/2013/coarsening_MST.pdf21 Jul 2013: 24–26]. To assess this issue, DICTRA simulations for coarsening with multicompo-nent diffusion and capillarity were carried out [27]. ... 24] D. E. Coates, Metallurgical Transactions 3 (1972) 1203–1212. [25] D. -
anisotropy
www.phase-trans.msm.cam.ac.uk/2013/anisotropy_Joo_ISIJ_2013.pdf19 Aug 2013: Reproduced from [24] with permission from Elsevier. Nonmetallic inclusions influence properties by nucleating cleavage or voids. ... Materials Science and Technology, 24:177–188, 2008. [74] S. Kotrechko, N. Stetsenko, and S. -
Theory for Hydrogen Desorptionin Ferritic Steel Eun Ju Song ...
www.phase-trans.msm.cam.ac.uk/2013/ferrite.pdf3 Jul 2013: Oriani’s model has been applied extensively to extract the apparent diffusiv-ity, trap density and binding energy from permeation experiments [15,21–24,for example]. ... Acta Materialia, 60:6814–6828, 2012. [24] J. Svoboda and F. D. Fisher. -
LTT3
www.phase-trans.msm.cam.ac.uk/2013/review_Ooi_MD_2014.pdf23 Dec 2013: been low [24] Martensitic Fe-Mn alloys can be very brittle [25-29] probably as a result of a co-. ... Fatigue and Fracture of Eng Mater. and Structures. 2008;31:125-36. [24] Martínez Díez F, Liu S. -
IOP PUBLISHING SCIENCE AND TECHNOLOGY OF ADVANCED MATERIALS Sci. ...
www.phase-trans.msm.cam.ac.uk/2013/first_Bhadeshia_STAM_2013.pdf16 Mar 2013: It has been known that the platelets of bainite becomethinner as the transformation temperature is reduced, andmodern analysis confirms this [23, 24]. ... Sci. Eng. A. A245 72[24] Hu F and Wu K 2011 Adv. -
paper wear.dvi
www.phase-trans.msm.cam.ac.uk/2013/Wear_Bakshi.pdf5 Nov 2013: 0.83 2.28 0.011 0.008 1.9 0.044 0.12 1.44 0.24 0.11 1.55 0.019 0.023. ... of thesteel [22–24], as opposed to when it is altered by changing the heat treatment for the samesteel [25]. -
The Bainite Controversy Lucy Fielding M.Eng. Department of Materials…
www.phase-trans.msm.cam.ac.uk/2013/controversy_Fielding_MST_2013.pdf4 Mar 2013: suggested that this initial case of mistaken identity influenced early theories of bainite formation [24, 25]. ... bainite [8]. After some further refinements [24, 46, 47] and comparison with experimental data [48, 49] it. -
02(2013-013).fm
www.phase-trans.msm.cam.ac.uk/2013/macro.pdf14 Jun 2013: The nucleation andstability of channel segregates were like- wise investigatedexperimentally and theoretically in a number of studies.24–26).
Search history
Recently clicked results
Recently clicked results
Your click history is empty.
Recent searches
Recent searches
Your search history is empty.