31 - 40 of 622 search results for TALK:PC53 20 |u:www.phase-trans.msm.cam.ac.uk where 0 match all words and 622 match some words.
  1. Results that match 1 of 2 words

  2. 050719_Italy 2005_Manuscript.DOC

    www.phase-trans.msm.cam.ac.uk/2005/LINK/156.pdf
    7 Jun 2010: 0 15 30 45 600.00. 0.05. 0.10. 0.15. 0.20. Frac. tion. ... 0.15. 0.20. 0.25. 0.30. 0.35. 0.40. 0.45. 0.50. 0.55. 0 1 2 3 4.
  3. 7 Jun 2010: IF–TiNb 3.3? 20 21 20 140 7 7 18 18 6.6 13 [5]. ... Advanced Engineering Materials,3:647–656, 2001. [20] G. Mukhopadhyay, S. Bhattacharya, and K.
  4. 1 Effect of Intergranular Ferrite on Hydrogen Delayed Fracture ...

    www.phase-trans.msm.cam.ac.uk/2005/LINK/66.pdf
    7 Jun 2010: Wt. % 0.20 0.056 0.1 0.004 0.004 0.04 0.004 0.04 0.317 43 30 Hot rolled bars with a diameter of 11mm were quenched ... A 0 1068 20 1787. B 6 1095 22 1754. C 10 1083 24 1710.
  5. FABRICATION AND WELDABILITY OF GRADE 23 TUBING AND PIPING ...

    www.phase-trans.msm.cam.ac.uk/2005/LINK/68.pdf
    7 Jun 2010: Tensile RT UTS > 510 MPa 641 (CW) 628 (CW) Weld metal 17 20. ... Tensile RT E > 20% 20.4 (AW) 23.1 (AW).
  6. ArcelorMittal Gerardy Buenos Aires

    www.phase-trans.msm.cam.ac.uk/2008/Highrise.pdf
    7 Jun 2010: 20. 30. 40. 50. 60. 70. 80. yiel. dst. reng. th[ k. ... 13/06/2007 ArcelorMittal Commercial Sections 20. Layout of the GREY millLayout of the GREY mill.
  7. Industrial Applications of the Mössbauer Effect, eds M. Garcia, ...

    www.phase-trans.msm.cam.ac.uk/2005/Mossbauer.pdf
    7 Jun 2010: The unusual properties are a consequence of the fine scale of the microstructure,which contains bainite plates with thickness in the range 20-40 nm. ... t site. s. Ferritic sites. Martensitic sites. Austenite. 20 40 60 80 100Annealing time (hours).
  8. Poster Plasticidad

    www.phase-trans.msm.cam.ac.uk/2002/mathew.poster.ppt
    7 Jun 2010: The toughness is in excess of 40 MPa m1/2 with upto 20% ductility tensile tests.
  9. Slide 1

    www.phase-trans.msm.cam.ac.uk/2005/TrendsPresentation.ppt
    7 Jun 2010: w. y. x. w. h. q. q. 00.050.10.150.20.25. C. N. B. ... Heat_Input. Preheat. Prep_Angle. PWHTtemp. PWHTtime. IPtest. TestTemp. log_tr. 0. 20. 40.
  10. (nanosteel.tex)

    www.phase-trans.msm.cam.ac.uk/2004/Tiny.pdf
    7 Jun 2010: By obtaining bainite in a strong austenitic steel at a largedriving force, it has been possible to obtain plates which are between 20–40 nm thick, resultingis steels which are ... Koiwa, K. Otsukaand T. Miyazaki, JIM (1999) 1533–36. 20. Hodgson PD,
  11. RELIABILITY OF COMPUTER SIMULATIONS FOR THE DESIGN OF A ...

    www.phase-trans.msm.cam.ac.uk/2005/LINK/123.pdf
    7 Jun 2010: The alloying elements have been varied as follows:. - 0.02 < C < 0.01 - 16 < Cr < 20 - 13 < Ni < 17 - 0 < Mo < 2 - 0.15 < N < 0.35. ... 0. 50. 100. 150. 200. 250. 300. 350. 400. 450. 18 20 22 24 26 28PLM (T273)(20logt)/1000.