Search

Search Funnelback University

Search powered by Funnelback
31 - 31 of 31 search results for katalk:za31 24 / / / / / |u:www.phase-trans.msm.cam.ac.uk where 0 match all words and 31 match some words.
  1. Results that match 1 of 2 words

  2. Thesis for Doctor of Philosophy Application of Lower Bainite ...

    www.phase-trans.msm.cam.ac.uk/2014/Thesis_ChaeJY.pdf
    6 Dec 2014: 52100 steel as illustrated in Figure 24 (Sakai 2002). 24. Figure 21: Schematic illustration of macroscopic fatigue fracture surface (Sachs. ... tempering temperature. The hardness of martensite for as-quenched, tempered at. 180, 230, and 250 conditions

Refine your results

Search history

Recently clicked results

Recently clicked results

Your click history is empty.

Recent searches

Recent searches

Your search history is empty.