  2. Effect of tempering upon the tensile properties of a novel bainitic…

    www.phase-trans.msm.cam.ac.uk/2014/Tempering.pptx
    31 Aug 2014: Austenite. 200. 17.3. 3.6218. 1.23. 220. 18.3. 3.6209. 1.23. 250. 21.4. ... Carbon / wt%. 200. 2.8721. 0.14. 220. 2.8706. 0.1. 250. 2.8621.
  3. Hydrogen_revised6

    www.phase-trans.msm.cam.ac.uk/2014/Han.pdf
    29 Mar 2014: 200. 400. 600. 800. 1000. Load. (µN. ). Displacement (nm). Non-charged H-charged. ... 0 50 100 150 200 2502.5. 2.8. 3.1. 3.4. 3.7. 4.0.
  4. Phase quantification in nanobainite via magnetic measurements and…

    www.phase-trans.msm.cam.ac.uk/2014/Magnetisation.pdf
    25 Nov 2014: Preprint submitted to Elsevier November 12, 2014. Journal of Magnetism and Magnetic Materials 378 (2015) 200-205. ... Samples were observed ina JEOL 200 CX with an accelerating voltage of 200 kV.
  5. tempering_Hasan_MSEA_2014

    www.phase-trans.msm.cam.ac.uk/2014/tempering_Hasan_MSEA_2014.pdf
    29 Aug 2014: DOI:10.1007/s40195-013-0006-2. 10. 400. 500. 600. 700. 0 50 100 150 200 250 300. ... γ{111}. γ{200} γ{113}γ{220}. 200oC. 220oC. 250oC. As-transformed. (b). 40 50 60 70 80 90 100.
  6. paperbainiterollingsliding.dvi

    www.phase-trans.msm.cam.ac.uk/2014/rolling_sliding.pdf
    21 May 2014: Heat Treatment Vickers hardness. 930 C 1h, air cooled to 200 C, held for 10 days, air cooled 622 13. ... Constant-depth nanoindentation was therefore used to tocharacterised changes on cross sections of the wear samples, prepared by polishing with 200
  7. Thesis for Doctor of Philosophy Hydrogen Desorption in Steels ...

    www.phase-trans.msm.cam.ac.uk/2014/thesis_EunJu.pdf
    6 Dec 2014: b) 100 C h1 and (c) 200 C h1. For all the curves,. ... undeformed and deformed sample with heating rate of (a). 100 and (b) 200 C h1.
  8. 18 Sep 2014: 250 Cwhich took around 6 min, introduced to an oven for isothermal heat treatmentat 200 C for 10 days, and cooled in air. ... These lamellae were then ob-served using a JEOL 200CX transmission electron microscope (TEM), withan accelerating voltage of 200
  9. October 14 WA Division Newsletter Page 4 Tool durability ...

    www.phase-trans.msm.cam.ac.uk/2014/WTIA_2014.pdf
    18 Oct 2014: Introducing what is considered a conservative value of 200 J mol-1 for the stored energy due to deformation (with refer-ence to studies of hot rolling of mild steels) into
  10. Hydrogen di↵usion and thepercolation of austenite in nanostructured…

    www.phase-trans.msm.cam.ac.uk/2014/percolation.pdf
    24 May 2014: Hydrogen diusion and thepercolation of austenite in. nanostructured bainitic steel. AUTHORS:Lucy Fielding a (corresponding author)Eun Ju Song b. Do-Kyeong Han b. Harshad Bhadeshia a,b. Dong-Woo Suh b. a Department of Materials Science and
  11. al_effect.dvi

    www.phase-trans.msm.cam.ac.uk/2014/al_effect.pdf
    13 Jul 2014: ENCUT 200 300 400 500 error. Eatom(Fe32), eV -8.222 -8.153 -8.144 -8.144 0.000.