Fully-matching results
-
Very Strong Low Temperature Bainite
www.phase-trans.msm.cam.ac.uk/2002/low.temperature.bainite.html14 Feb 2020: Very Strong Low Temperature Bainite. F. G. Caballero, H. K. D. H. Bhadeshia, K. J. A. Mawella, D. G. Jones and P. Brown. Abstract. Bainite has been obtained by heat treatment at temperatures as low as 125. o. C in a high carbon, high silicon steel. -
Slide Presentations
www.phase-trans.msm.cam.ac.uk/2001/slides.html10 Jul 2024: Slide presentations. Automotive Steels. Bainite. POSCO Lectures on Bainite. Bainitic pipe. Cologne 2014. Percolation of phases, MST 2015. Buildings. Cast Iron. Austempered ductile cast iron. Carbides. Creep. Crystallography. Diffusion. Dispersion -
Acceleration of Low-Temperature Bainite
www.phase-trans.msm.cam.ac.uk/2003/fast.bainite.html14 Feb 2020: Acceleration of Low-Temperature Bainite. C. Garcia Mateo, F. G. Caballero and H. K. D. H. Bhadeshia. Abstract. Recent work has shown that bainitic ferrite plates produced by transformation at low temperatures can be as thin as 20 nm with a hardness -
Properties of Fine-Grained Steels Generated by Displacive…
www.phase-trans.msm.cam.ac.uk/2008/fine.html14 Feb 2020: Properties of Fine-Grained Steels Generated by Displacive Transformation. H. K. D. H. Bhadeshia. Abstract. It has been possible in recent times to make large quantities of steels in which the controlling scale is 20 nm or less, i.e., comparable to -
A Personal Commentary on "Transformation of Austenite at…
www.phase-trans.msm.cam.ac.uk/2010/Bain.html14 Feb 2020: Download PDF file of paper, with permission from TMS International. -
Mechanical stabilisation of austenite
www.phase-trans.msm.cam.ac.uk/2006/stabilisation.html14 Feb 2020: Mechanical stabilisation of austenite. S. Chatterjee, H. S. Wang, J. R. Yang and H. K. D. H. Bhadeshia. Abstract. A theory has been developed for the mechanical stabilisation of plastically deformed austenite by balancing the force which drives the -
Surface Relief due to Bainite
www.phase-trans.msm.cam.ac.uk/abstracts/swallow.html14 Feb 2020: High resolution observations of displacements caused by bainitic transformation. E. Swallow and H. K. D. H. Bhadeshia, University of Cambridge. Abstract. High resolution measurements of the displacements caused by the formation of bainite in a steel -
Effect of 30 Tesla Magnetic Field on Transformations in a Novel…
www.phase-trans.msm.cam.ac.uk/2004/magnet.html14 Feb 2020: Effect of 30 Tesla Magnetic Field on Transformations in a Novel Bainitic Steel. R. A. Jaramillo, S. S. Babu, G. M. Ludtka, R. A. Kisner, J. B. Wilgen, G. Mackiewicz-Ludtka, D. M. Nicholson, S. M. Kelly, M. Murugananth and H. K. D. H. Bhadeshia. -
Mechanically Alloyed Metals
www.phase-trans.msm.cam.ac.uk/2000/cirencester.html14 Feb 2020: Mechanically Alloyed Metals. H. K. D. H. Bhadeshia. Abstract. Mechanical alloying involves the severe deformation of mixtures of powders until they form the most intimate of atomic solutions. Inert oxides can also be introduced to form a uniform -
Crystallographic Texture of Stress-Affected Bainite
www.phase-trans.msm.cam.ac.uk/2007/texture_bainite.html14 Feb 2020: Crystallographic Texture of Stress-Affected Bainite. S. Kundu, K. Hase and H. K. D. H. Bhadeshia. Abstract. A method is presented for calculating both the macroscopic strains and crystallographic bias which develop when a polycrystalline sample of
Refine your results
Date
- 343 2020
- 263 2010
- 58 2017
- 8 Past 3 months
- 8 Past month
- 8 Past 6 months
- 8 2024
- 8 Past year
- 3 2021
- 1 2012
- 1 2022
- 1 2011
Search history
Recently clicked results
Recently clicked results
Your click history is empty.
Recent searches
Recent searches
Your search history is empty.