Hydrogen di↵usion and thepercolation of austenite in nanostructured…
www.phase-trans.msm.cam.ac.uk/2014/percolation.pdf24 May 2014: was measured using quantitative X-rayanalysis. After tempering, the samples were ground with progressively finergrades of silicon carbide paper, up to 4000 grit. ... Therefore, the appropriate D. is that measured using per-meation experiments on this