Fully-matching results
-
Materials Science Forum, 500–501 (2005) 63–74. High Performance…
www.phase-trans.msm.cam.ac.uk/2005/performance.pdf7 Jun 2010: It is shown in this paper that the theory of bainite can be used to create exciting alloys.The examples discussed cover rails and protective armour; others are discussed elsewhere [5]. -
Christmas
www.phase-trans.msm.cam.ac.uk/2009/stainless_Abreu_MR_2009.pdf7 Jun 2010: Texture analysis of deformation induced martensite in an AISI 301L stainless steel: microtexture and macrotexture aspects. Hamilton Ferreira Gomes de AbreuI, ; Marcelo José Gomes da SilvaI; Luís Flávio Gaspar HerculanoI; H. BhadeshiaII. -
Current Opinion in Solid State and Materials Science 8 ...
www.phase-trans.msm.cam.ac.uk/2005/current.pdf7 Jun 2010: Current Opinion in Solid State and Materials Science 8 (2004) 251-257. Very Strong Bainite. F. G. Caballero a and H. K. D. H Bhadeshia b. a Department of Physical Metallurgy, Centro Nacional de Investigaciones Metalúrgicas(CENIM), Consejo Superior -
Austenite films in bainitic microstructuresL. C. Chang and H. ...
www.phase-trans.msm.cam.ac.uk/2008/film.pdf7 Jun 2010: OPTICAL AND TRANSMISSION ELECTRONMICROSCOPYThe specimens were prepared for optical microscopy bymounting in conductive Bakelite, grinding using 120 gritsilicon carbide paper, and finally, polishing down to 1 /lmdiamond grit. ... However,much of the work -
Critical assessment: friction stir welding ofsteels H. K. D. ...
www.phase-trans.msm.cam.ac.uk/2009/critical_STWJ_2009.pdf7 Jun 2010: This paper raises a few important issues. The modelincludes the calculation of the temperature distributioninside the tool. ... Schneider: In ‘SAE technical paper series’, 1–6;. 1992, Warrendale, PA, Society of Automobile Engineers. -
Induction welding and heat treatment of steelpipes: evolution of ...
www.phase-trans.msm.cam.ac.uk/2010/pipe_Yan_STWJ_2010.pdf7 Jun 2010: All the samples were cut normalto the welding direction which is parallel to the rollingdirection, which in turn is parallel to the pipe axis.Samples were then ground using sand paper, -
Solid→Solid Phase Transformations in Inorganic Materials Edited by J. …
www.phase-trans.msm.cam.ac.uk/2006/PTM05.pdf7 Jun 2010: The purpose of this paper is to describe the currentunderstanding of this novel hard bainite in terms of atomic mechanisms, thermodynamicsand structure–property relationships. ... After D. Crowther and P. Brown. Summary. There are many adjectives that -
Investigations Into the Microstructure: Toughness Relation in High…
www.phase-trans.msm.cam.ac.uk/2010/IPC2010-31372.pdf8 Oct 2010: ArcelorMittal Commercial FCE Fos-sur-Mer, France. In the present paper, investigations performed on ArcelorMittal X65 linepipe steel in order to understand the effects of high frequency induction (HFI) welding process ... Pipeline Technology Conference -
Cottrell_ICFRM12(2)
www.phase-trans.msm.cam.ac.uk/2007/Charpy_Cottrell_JNM_2007.pdf7 Jun 2010: highlights the problems of extrapolation and interpolation. This paper describes development of a Neural Network (NN) model for the ductile-. -
superbainite_strain.dvi
www.phase-trans.msm.cam.ac.uk/2009/superbainite_strain.pdf7 Jun 2010: Bainite Orientation in Plastically Deformed Austenite. International Journal of Materials Research 100 (2009) 40-45. A. A. Shirzadi, H. Abreu‡, L. Pocock,D. Klobc̆ar†, P. J. Withers and H. K. D. H. Bhadeshia. University of Cambridge, Materials