  2. Low Temperature Bainite

    www.phase-trans.msm.cam.ac.uk/2002/mateo.html
    14 Feb 2020: Journal de Physique IV, Vol. 112 (2003) 17-25. High-resolution Images (TIFF).
  3. Silicon-Rich Bainitic Steel Welds

    www.phase-trans.msm.cam.ac.uk/2003/Lord.Silicon.html
    14 Feb 2020: Download PDF file of paper. ... High Resolution Images. Slides.
  4. Bainite in Steels

    www.phase-trans.msm.cam.ac.uk/bainite_NN.html
    22 Dec 2022: Bainite in Steels. Free books available for download. Zhinan Yang, Fucheng Zhang.
  5. Bainitic seamless pipes

    www.phase-trans.msm.cam.ac.uk/2009/gomez1.html
    14 Feb 2020: Air-Cooled Bainitic Steels for Strong, Seamless Pipes Part 1: Alloy Design, Kinetics and Microstructure. G. Gomez, T. Pérez and H. K. D. H. Bhadeshia. Abstract. Seamless pipes are usually quenched and tempered after manufacture in order to obtain
  6. Tempering of a Hard Mixture of Bainitic Ferrite and Austenite

    www.phase-trans.msm.cam.ac.uk/2004/bainite.tempering.html
    14 Feb 2020: Book on bainite (electronic version available for free download). Movies about Martensite and Bainite.
  7. 14 Feb 2020: White-etching matter in bearing steel. Part 1: Controlled-cracking of bearing steel. W. Solano-Alvarez and H. K. D. H. Bhadeshia. Abstract. Although most of the research performed in steel metallurgy aims to prevent crack nucleation and propagation,
  8. Atomic mechanism of the bainite transformation

    www.phase-trans.msm.cam.ac.uk/2018/mechanism.html
    14 Feb 2020: Atomic mechanism of the bainite transformation. H. K. D. H. Bhadeshia. Abstract. I have on previous occasions shown how we can be surprised and delighted by new discoveries in steels, which at the same time may be useful. However, my focus in this
  9. Hard Bainite

    www.phase-trans.msm.cam.ac.uk/2003/hard.bainite.html
    14 Feb 2020: ISIJ International, 43 (2003) 1238-1243. High-resolution Images (TIFF). Bainitic Phase Transformations.
  10. Very Strong Low Temperature Bainite

    www.phase-trans.msm.cam.ac.uk/2002/low.temperature.bainite.html
    14 Feb 2020: Materials Science and Technology, 18 (2002) 279-284. High-resolution Images (TIFF). Bainitic Phase Transformations.
  11. Acceleration of Low-Temperature Bainite

    www.phase-trans.msm.cam.ac.uk/2003/fast.bainite.html
    14 Feb 2020: ISIJ International, 43 (2003) 1821-1825. High-resolution Images (TIFF). Bainitic Phase Transformations.