www.phase-trans.msm.cam.ac.uk/2016/preventing_hydrogen.pdf18 Jan 2016: Prevention of Hydrogen Embrittlement in Steels. H. K. D. H. Bhadeshiaa. aMaterials Science and Metallurgy, University of Cambridge, U.K. Abstract. The essential facts about the nature of the hydrogen embrittlement of steelshave now been known for