Fully-matching results
-
Pure, amorphous iron
www.phase-trans.msm.cam.ac.uk/2024/amorphous.html6 Jul 2024: Pure, amorphous iron. H. K. D. H. Bhadeshia. Abstract. The review covers the difficulty in obtaining amorphous iron, the clever experiments that have produced small particles or thin films of glassy iron, together with models that estimate the -
Martensite and Martensitic Phase Transformations
www.phase-trans.msm.cam.ac.uk/2002/martensite.html4 Jul 2024: Martensite and Martensitic Phase Transformations. H. K. D. H. Bhadeshia. Evolution of martensite. A movie of martensitic transformation in Fe-0.18C-0.2Si-0.9Mn-2.9Ni-1.5Cr-0.4Mo wt% steel, using confocal laser microscopy. The time and temperature -
Retained Austenite
www.phase-trans.msm.cam.ac.uk/2004/retained.austenite.html4 Jul 2024: Retained Austenite. Crystallography of Austenite. Theory and Significance of Retained Austenite in Steels. Ph.D. thesis, by Harry Bhadeshia, University of Cambridge, 1979. Reaustenitisation of some Alloy Steels. Ph.D. thesis, by Ursula Ruth Lenel, -
Teaching Metallurgy
www.phase-trans.msm.cam.ac.uk/teaching.html4 Jul 2024: Teaching Materials. H. K. D. H. Bhadeshia.. Crystallography. Examination questions. Slides and Videos. Animations. Scaleable vector graphics. Metals & Alloys (year 2). Phase transformations (year 2, Queen Mary University of London). Phase -
Current Opinion in Solid State and Materials Science Special Issue on …
www.phase-trans.msm.cam.ac.uk/2005/special.html7 Jul 2024: Current Opinion in Solid State and Materials Science, Special Issue on Bainite, Volume 8, 2004. Bainite Transformations (Preface). Pages 211 to 211. Bhadeshia, Harry. Recent progress: kinetics of the bainite transformation in steels. Pages 213 to -
Cast irons
www.phase-trans.msm.cam.ac.uk/2001/adi/cast.iron.html4 Jul 2024: Cast Irons. Miguel Angel Yescas-Gonzalez and H. K. D. H. Bhadeshia. Cast irons typically contain 2-4 wt% of carbon with a high silicon concentrations and a greater concentration of impurities than steels. The carbon equivalent (CE) of a cast iron -
Nickel Based Superalloys
www.phase-trans.msm.cam.ac.uk/2003/Superalloys/superalloys.html4 Jul 2024: Nickel Based Superalloys. H. K. D. H. Bhadeshia. A superalloy is a metallic alloy which can be used at high temperatures, often in excess of 0.7 of the absolute melting temperature. Creep and oxidation resistance are the prime design criteria. -
Tempered Martensite
www.phase-trans.msm.cam.ac.uk/2004/Tempered.Martensite/tempered.martensite.html4 Jul 2024: Tempered Martensite. H. K. D. H. Bhadeshia. Introduction. Tempering is a term historically associated with the heat treatment of martensite in steels. It describes how the microstructure and mechanical properties change as the metastable sample is -
Stainless Steels
www.phase-trans.msm.cam.ac.uk/2005/Stainless_steels/stainless.html4 Jul 2024: Stainless Steels. T. Sourmail and H. K. D. H. Bhadeshia. Introduction. Steels are said to be stainless when they resist corrosion; the is achieved by dissolving sufficient chromium in the iron to produce a coherent, adherent, insulating and