Search

Search Funnelback University

Search powered by Funnelback
1 - 15 of 15 search results for download |u:www.phase-trans.msm.cam.ac.uk
  1. Fully-matching results

  2. Phase Transformations and Complex Properties

    www.phase-trans.msm.cam.ac.uk/
    16 Jun 2024: Phase Transformations & Complex. Properties Research Group. Queen Mary University of London. Emeritus Tata Steel Professor of Metallurgy. University of Cambridge. Ph.D. student. Rajdeep Mondal. rajdeep.mondal@qmul.ac.uk. Honorary Associates. The
  3. Phase Transformations and Complex Properties

    www.phase-trans.msm.cam.ac.uk/index.html
    16 Jun 2024: Phase Transformations & Complex. Properties Research Group. Queen Mary University of London. Emeritus Tata Steel Professor of Metallurgy. University of Cambridge. Ph.D. student. Rajdeep Mondal. rajdeep.mondal@qmul.ac.uk. Honorary Associates. The
  4. Continuously cooled hypoeutectoid steel

    www.phase-trans.msm.cam.ac.uk/2011/mixed/index.html
    24 Jun 2024: Continuously cooled hypoeutectoid steel. H. K. D. H. Bhadeshia. The vast majority of the 1.3 billion tonnes of steel proudced annually have a microstructure which is a mixture of allotriomorphic ferrite and pearlite. The pearlite is the last phase
  5. Steels for rails

    www.phase-trans.msm.cam.ac.uk/2024/rail.html
    28 Jun 2024: Steels for rails. W. Solano-Alvarez and H. K. D. H. Bhadeshia. Abstract. Transport by rail is an efficient way of moving goods and people while managing problems such as congestion and the consequences on the environment. The relatively low energy
  6. Martensite and Martensitic Phase Transformations

    www.phase-trans.msm.cam.ac.uk/2002/martensite.html
    4 Jul 2024: Martensite and Martensitic Phase Transformations. H. K. D. H. Bhadeshia. Evolution of martensite. A movie of martensitic transformation in Fe-0.18C-0.2Si-0.9Mn-2.9Ni-1.5Cr-0.4Mo wt% steel, using confocal laser microscopy. The time and temperature
  7. Phase Transformations and Complex Properties Research Group

    www.phase-trans.msm.cam.ac.uk/books.html
    14 Jun 2024: Books. Available for Free Download. The following reproduced with the permission of Dr Alan Armour, Climax Molybdenum. ... Restricted Download. Published, 2023. October 8th, 2024.
  8. Retained Austenite

    www.phase-trans.msm.cam.ac.uk/2004/retained.austenite.html
    4 Jul 2024: Retained Austenite. Crystallography of Austenite. Theory and Significance of Retained Austenite in Steels. Ph.D. thesis, by Harry Bhadeshia, University of Cambridge, 1979. Reaustenitisation of some Alloy Steels. Ph.D. thesis, by Ursula Ruth Lenel,
  9. Teaching Metallurgy

    www.phase-trans.msm.cam.ac.uk/teaching.html
    4 Jul 2024: Teaching Materials. H. K. D. H. Bhadeshia.. Crystallography. Examination questions. Slides and Videos. Animations. Scaleable vector graphics. Metals & Alloys (year 2). Phase transformations (year 2, Queen Mary University of London). Phase
  10. Cast irons

    www.phase-trans.msm.cam.ac.uk/2001/adi/cast.iron.html
    4 Jul 2024: Cast Irons. Miguel Angel Yescas-Gonzalez and H. K. D. H. Bhadeshia. Cast irons typically contain 2-4 wt% of carbon with a high silicon concentrations and a greater concentration of impurities than steels. The carbon equivalent (CE) of a cast iron
  11. MAP_STEEL_AUSTENITEGROWTH

    www.phase-trans.msm.cam.ac.uk/map/steel/programs/austenitegrowth.html
    31 Jan 2024: H. Bhadeshia, 2024, the relevant page of which is included in the download files. ... steel, pearlite, austenite, austenite growth, kinetics. Download.
  12. Nickel Based Superalloys

    www.phase-trans.msm.cam.ac.uk/2003/Superalloys/superalloys.html
    4 Jul 2024: Nickel Based Superalloys. H. K. D. H. Bhadeshia. A superalloy is a metallic alloy which can be used at high temperatures, often in excess of 0.7 of the absolute melting temperature. Creep and oxidation resistance are the prime design criteria.
  13. Phase Transformations and Complex Properties Research Group

    www.phase-trans.msm.cam.ac.uk/2000/phd.html
    15 Apr 2024: Mitigating high-temperature, high-pressure hydrogen attack. Ph.D. thesis, by Mohammed Abdulrahman Alshahrani, University of Cambridge, 2021. Role of toughness in abrasion and impact-abrasion wear. Ph.D. thesis, by Appa Rao Chintha, University of
  14. Metallography of Steels

    www.phase-trans.msm.cam.ac.uk/2008/Steel_Microstructure/SM.html
    24 Jun 2024: You can freely download the complete book Theory of Transformations in Steels.
  15. Tempered Martensite

    www.phase-trans.msm.cam.ac.uk/2004/Tempered.Martensite/tempered.martensite.html
    4 Jul 2024: Tempered Martensite. H. K. D. H. Bhadeshia. Introduction. Tempering is a term historically associated with the heat treatment of martensite in steels. It describes how the microstructure and mechanical properties change as the metastable sample is
  16. Stainless Steels

    www.phase-trans.msm.cam.ac.uk/2005/Stainless_steels/stainless.html
    4 Jul 2024: Stainless Steels. T. Sourmail and H. K. D. H. Bhadeshia. Introduction. Steels are said to be stainless when they resist corrosion; the is achieved by dissolving sufficient chromium in the iron to produce a coherent, adherent, insulating and