  2. Review: friction stir welding tools R. Rai1, A. De2, ...

    www.phase-trans.msm.cam.ac.uk/2011/tools_Rai_STWJ_2011.pdf
    14 Apr 2011: Review: friction stir welding tools. R. Rai1, A. De2, H. K. D. H. Bhadeshia3 and T. DebRoy1. Friction stir welding (FSW) is a widely used solid state joining process for soft materials such as. aluminium alloys because it avoids many of the common