  2. TOWARDS ECONOMIC DESIGN OF A PRESSURE VESSEL MADE OF ...

    www.phase-trans.msm.cam.ac.uk/2005/LINK/99.pdf
    7 Jun 2010: Stre. ss [M. Pa]. ref_test_Tref_test_L. Fig. 1 Comparison of stress-strain relation between coupon tests along. ... Welded test specimen, especially tests with butt welds show greater variation between results.
  3. Materials Science & Metallurgy Master of Philosophy, Materials…

    www.phase-trans.msm.cam.ac.uk/mphil/MP9.EX2.pdf
    7 Jun 2010: should remain. within the European Economic Community. At the time, 52% of the electorate. ... 40%. of your accumulated test data come from machine A. Find the probability that a.
  4. (Davies.Automobile)

    www.phase-trans.msm.cam.ac.uk/2003/Geoff.Davies.pdf
    7 Jun 2010: of the subject, incorporating aspects of science, engineering and economics. The entire range. ... a proper discussion of dent–resistance and the test used to characterise this largely aesthetic.
  5. COMPLEX MECHANICAL PROPERTIES OF STEEL Radu Calin Dimitriu Department …

    www.phase-trans.msm.cam.ac.uk/2009/Radu_Thesis.pdf
    7 Jun 2010: d average grain size. E elastic modulus. ED test error. EE calculated error. ... tensile test. The rate of this deformation is a function of the material.
  6. Final draft

    www.phase-trans.msm.cam.ac.uk/2008/Minsung_Thesis.pdf
    7 Jun 2010: the Charpy toughness tests. The Charpy impact test is a standardized high strain-rate test which determines the. ... test because it is simple, inexpensive and nondestructive. There are many kinds of tests to evaluate hardness for the materials.
  7. Alloy Design for a Fusion Power Plant Richard Kemp ...

    www.phase-trans.msm.cam.ac.uk/2006/Kemp.thesis.pdf
    7 Jun 2010: xi. Term Meaning. Tirr Irradiation temperatureTtest Tensile test temperatureQ Activation energy for an Arrhenius processk Boltzmann’s constant. ... economics. Table 2.2: Functions and requirements of a fusion power-plant blanket structure.
  8. Microstructure evolution in irons and steels:a tribute to David ...

    www.phase-trans.msm.cam.ac.uk/2010/IHT467.pdf
    25 Jun 2010: He was recruited toOxford in part to help create the MEM (Metallurgy,Economics and Management) programme, designed tonurture captains of engineering industry. ... the strain-rate range 103 to.1025 s21, achieved by Hopkinson bar tests andexplosively
  9. 1 THE APPLICATION OF HIGH-ALLOYED STEEL IN VEHICLE STRUCTURES ...

    www.phase-trans.msm.cam.ac.uk/2005/LINK/115.pdf
    7 Jun 2010: to a road test, it was necessary to build a drivable experimental spaceframe for systematic tests using thermal joining (welding). ... Performance of preliminary tests to secure the technology and determine the joining parameters.
  10. 1 DEVELOPMENT OF NEW IN-MILL MECHANICAL TESTING TOWARDS X100 ...

    www.phase-trans.msm.cam.ac.uk/2005/LINK/140.pdf
    7 Jun 2010: A way of bridging between mill acceptance tests and field situation is proposed. ... 1. STATE OF THE ART Acceptance tests and their use Classically, the Charpy V Notch test (CVN) is used to qualify a pipe regarding crack failure risk.
  11. ACKNOWLEDGEMENTS I would like to thank my supervisor Professor ...

    www.phase-trans.msm.cam.ac.uk/2003/fabien.report.pdf
    7 Jun 2010: Figure 1.3 shows results after a classical long-term creep-resistance test for a few steels. ... The picture at the right is for a short-term creep test [5].
  12. Thesis (June98)

    www.phase-trans.msm.cam.ac.uk/2008/Shirzadi_Thesis.pdf
    7 Jun 2010: Chapter 1 Introduction. 2. advanced aluminium-based materials, the lack of a reliable and economic joining. ... 1996). conducted tensile tests on miniature Al-Li 8090 bonds. A scanning Auger microprobe.
  13. Master Thesis Thermodynamic Study on B and Fe Substituted ...

    www.phase-trans.msm.cam.ac.uk/2010/Young_Thesis.pdf
    2 Jul 2010: economic and environmental aspects. The efficiency of steam power plants nowadays is around with a steam. ... until failure or rupture appears occurs in constant load creep tests at high stresses.
  14. Influence of carbon, manganese and nickel onmicrostructure and…

    www.phase-trans.msm.cam.ac.uk/2006/Coalesced.1.Keehan.STWJ.2006.pdf
    7 Jun 2010: These weld metals have hadlimited use, primarily owing to economic factors and lackof flexibility. ... 1998–1999. 15. ‘Charpy impact test on metallic materials; part 1: test method’,.
  15. A Tribute to Professor David V. Edmonds on the Eve of His Retirement

    www.phase-trans.msm.cam.ac.uk/2009/MST/edmonds.pdf
    7 Jun 2010: Anne’s College. He was recruited to Oxford in part to help create the MEM program (“Metallurgy, Economics and Management”), designed to nurture captains of engineering industry. ... indicating percolated nature of the microstructure [93]. BCC iron
  16. 1 TECHNOLOGICAL SOLUTIONS FOR ULTRA-HIGH STRENGTH GAS PIPELINES Dr.…

    www.phase-trans.msm.cam.ac.uk/2005/LINK/174.pdf
    7 Jun 2010: The tests were performed on strip specimen at ambient temperature. The statistics are based on 56 individual test results. ... But the economic transport of gas over very long distances requires additional cost cuts.
  17. 7 Jun 2010: Small-scale tensile tests, ring expansion test, and hydrostatic burst test were conducted to ensure the tensile properties of high strength line pipe steel against internal pressure. ... 2-2. Welded joint tensile test results. Welded joint tensile tests
  18. PowerPoint Presentation - 1998 overtime hours

    www.phase-trans.msm.cam.ac.uk/2005/RR/RR_files/RR.ppt
    7 Jun 2010: type test). Overall. pressure. ratio. 1970s. 1980s. 1990s. 2000. Cruise SFC v OPR & TET. ... T890. T895. T772. 1975. 2000. 1300. 1600. Type test temperatures of RB211 & Trent HP turbine blades.
  19. 1 PRODUCTION AND APPLICATION OF HIGH STRENGTH STEEL Feng ...

    www.phase-trans.msm.cam.ac.uk/2005/LINK/33.pdf
    7 Jun 2010: Table 2 Mechanical properties with different process Tensile Test Impact Test Bending. ... Fig 1 shows some application cases. 2.3 ECONOMIC EFFECTS Table 3 shows the material saving results of one high strength steel substituted the other lower strength
  20. paper46

    www.phase-trans.msm.cam.ac.uk/2005/LINK/46.pdf
    7 Jun 2010: The delivery conditions in EN 10149 do not include a mandatory test of impact energy. ... Test specimen “O“. Test specimen “S“. Fig.10. Structural detailing and large scale specimens.
  21. THE DESIGN OF X80 TO X120 STEELS WITH INCREASED ...

    www.phase-trans.msm.cam.ac.uk/2005/LINK/119.pdf
    7 Jun 2010: Additional details can be found in [6]. In all corrosion tests the pH was continually monitored throughout each test run and was controlled by the partial pressure of the CO2, this ... The test temperature was maintained at 303K (30oC) throughout. In