Cracks in martensite plates as hydrogen traps in a ...
www.phase-trans.msm.cam.ac.uk/2015/Hydrogen_cracks.pdf17 Jan 2015: 2.6. Electrochemical Hydrogen Permeation. Using a Devanathan and Stachurski cell, hydrogen permeation tests atroom temperature were conducted according to ISO 17081-2004 standard[22, 23]. ... The eect of hydrogen. 12. Table 4: Parameters determined