  2. histogramX65148_paper2.eps

    www.phase-trans.msm.cam.ac.uk/2011/frequency.pdf
    13 Oct 2011: In the middle of the weld junction, the M–A islands are alignedalong the normal direction (Fig. ... RD–TD surfaces with the weld junctionin the middle were prepared for investigation of inclusions.
  3. template.dvi

    www.phase-trans.msm.cam.ac.uk/2011/transfer_Hasan_2011.pdf
    18 Feb 2011: probe test. In: Wallis RA, Walton HW (eds) Heat Treating: Proceedings of the. ... b) Comparison between calculatedand measured hardness values. The top and middle sets of points represent the Inconel andJIS probes respectively, and the measured values
  4. Review: friction stir welding tools R. Rai1, A. De2, ...

    www.phase-trans.msm.cam.ac.uk/2011/tools_Rai_STWJ_2011.pdf
    14 Apr 2011: degradation and process economics. Keywords: Friction stir welding, Tool material, Tool geometry, Load bearing ability. ... Inmodel tests, diffusion couples of pcBN and 100Cr6 wereexposed to 1223 K for 20 h followed by abrasion ofpcBN surfaces with a
  5. 4th draft

    www.phase-trans.msm.cam.ac.uk/2011/PhD_Thesis_Yang.pdf
    29 Sep 2011: 24. from elastic deformation. In the case of a tensile test, it is conventional to offset the. ... test line by a strain of 0.2 % in order to define the proof strength.