  2. paper.dvi

    www.phase-trans.msm.cam.ac.uk/2010/extraordinary.pdf
    24 Nov 2010: The isothermal transformation caneven be conducted at 450C which is compatible with a final galvanising treatment. ... Theauthors are also grateful for support from the World Class University Programmeof the National Research Foundation of Korea,
  3. TMS_Modified

    www.phase-trans.msm.cam.ac.uk/2008/synchrotron_Dai_MTA_2008.pdf
    7 Jun 2010: However, where solid state transformations occur during the welding process it can be difficult to ascertain how the stress distribution evolved solely from an examination of the final weld. ... 1981. [16]. S. M. Hodson: “MTDATA-Metallurgical and
  4. doi:10.1016/j.calphad.2003.08.002

    www.phase-trans.msm.cam.ac.uk/2003/Multiple.precipitation.pdf
    7 Jun 2010: It should be noted that the behaviour and final amountof phases are dictated by the underlying thermodynamicmodels. ... However, examination of thedifferent micrographiespublished in [20] revealed considerable difference in grainsizes between 304 and 347.
  5. Influence of carbon, manganese and nickel onmicrostructure and…

    www.phase-trans.msm.cam.ac.uk/2006/Coalesced.1.Keehan.STWJ.2006.pdf
    7 Jun 2010: These weld metals have hadlimited use, primarily owing to economic factors and lackof flexibility. ... ALeitz Aristomet LOM, a Philips XL30 SEM, and a LeoUltra 55 FEGSEM were used in these examinations.For transmission electron microscopy (TEM) studies,.
  6. A Tribute to Professor David V. Edmonds on the Eve of His Retirement

    www.phase-trans.msm.cam.ac.uk/2009/MST/edmonds.pdf
    7 Jun 2010: influence final microstructure; Si, Ni and Cu graphitisers in the eutectic cell, and Mn, Mo carbide promoters in intercellular regions. ... Paetke and D.V. Edmonds, Deformation of Polycrystals: Materials and Microstructure, Riso National Laboratory,
  7. THE DEVELOPMENT OF ULTRAHIGH STRENGTH WIRE Shaun Hobson – ...

    www.phase-trans.msm.cam.ac.uk/2005/LINK/6.pdf
    7 Jun 2010: The detailed property requirements for high strength galvanised wire depend on the final application and are usually specified by the customer. ... Therefore, this steel chemistry was selected as the base composition for a detailed examination, initially
  8. AA SSttuuddyy of the OOxxyyggeennaattiioonn and…

    www.phase-trans.msm.cam.ac.uk/2004/Ti-6Al-4V.pdf
    7 Jun 2010: Before commencing the homogenisation, the programs calculate the mean concentration. This is re-calculated from the final values after the homogenisation has taken place. ... 7. H. E. Swanson, R. K. Fuyat & G. M. Ugrinic: National Bureau of Standards (U.S
  9. template.dvi

    www.phase-trans.msm.cam.ac.uk/2010/dual_Kim.pdf
    22 Jul 2010: the final microstructure, permitting its crystallographic orientation to be determined. without ambiguity. ... using microhardness indents for further examination in a scanning electron microscope.
  10. Thesis (June98)

    www.phase-trans.msm.cam.ac.uk/2008/Shirzadi_Thesis.pdf
    7 Jun 2010: Chapter 1 Introduction. 2. advanced aluminium-based materials, the lack of a reliable and economic joining. ... materials in air is reviewed in the final section. The experimental procedures for the.
  11. 1 MANUFACTURING AND MECHANICAL & METALLURGICAL PROPERTIES OF 9 ...

    www.phase-trans.msm.cam.ac.uk/2005/LINK/100.pdf
    7 Jun 2010: Ingot Making. Melting. P.H.T. ESR. Q.H.T. Machining. Final Inspection. U.T. 8. ... a) Surface b) Middle c) Center. Ultrasonic examination was done on the machined rotor.
  12. COMPLEX MECHANICAL PROPERTIES OF STEEL Radu Calin Dimitriu Department …

    www.phase-trans.msm.cam.ac.uk/2009/Radu_Thesis.pdf
    7 Jun 2010: COMPLEX MECHANICAL. PROPERTIES OF STEEL. Radu Calin Dimitriu. Department of Materials Science and Metallurgy. University of Cambridge. Churchill College. A dissertation submitted for thedegree of Doctor of Philosophy. at the University of
  13. B5 final

    www.phase-trans.msm.cam.ac.uk/2007/Yang_Thesis.pdf
    7 Jun 2010: i. Master Thesis. Low-Carbon, Low-Temperature Bainite. Yang, Hong-Seok ( 梁 洪 碩 ). Department of Ferrous Technology. (Computational Metallurgy). Graduate Institute of Ferrous Technology. Pohang University of Science and Technology. 2008. ii.
  14. Preface

    www.phase-trans.msm.cam.ac.uk/2003/shen.thesis.pdf
    7 Jun 2010: examination of the weights [12]. A better method is to actually use the network to make. ... The final output y (dependent variable) is defined as below [22]:.
  15. Paper4.indd

    www.phase-trans.msm.cam.ac.uk/2005/Enda/Paper4.pdf
    7 Jun 2010: These weld metals have had limited use primarily due to economic fac-tors and lack of flexibility. ... At larger concentrations it increases the preservation of retained austenite in the final microstructure.
  16. The Kirkendall Effect in Solid State Diffusion PhD Thesis ...

    www.phase-trans.msm.cam.ac.uk/2004/Kirkendall.Aloke.pdf
    7 Jun 2010: Chapter 2. impregnated discs. After that, final polishing of the surfaces was performed by 0.5 µm alumina slurry. ... from the examination of the Kirkendall marker shift in the reaction couples listed in Table (3.1-1) are displayed graphically.
  17. δ-T RIP Ste el 2 010 Y i, Honglia ...

    www.phase-trans.msm.cam.ac.uk/2010/Yi_Thesis.pdf
    1 Jul 2010: composition, processing and heat treatment, all of which lead to its final microstructure. ... final part. It transforms into martensite during subsequent deformation, such as during.
  18. The use of very high strength steels

    www.phase-trans.msm.cam.ac.uk/2005/LINK/189.pdf
    7 Jun 2010: US-StandardsASTM. European Committee for Standardization (CEN). Commission of the European CommunitiesEuropean National Standard Bodies. ... 3.4 Stability (1) There are two limit states that may adversely affect the economic exploitation of the.
  19. M. A. Yescas*University of Cambridge, Department of Materials Science …

    www.phase-trans.msm.cam.ac.uk/2005/adi.Yescas.CMR.2003.pdf
    7 Jun 2010: Thus, a shorttime leads to a final microstructure which is predomi-nantly martensitic and very hard. ... Storesun and R. Sandstrom, 2nd Inter.;. national Conference on Austempered Ductile Iron, 17-19March, University of Michigan Ann Arbor, Michigan,
  20. THE TAP PROJECT F. Marchesani, E. Donati – Snamprogetti, ...

    www.phase-trans.msm.cam.ac.uk/2005/LINK/186.pdf
    7 Jun 2010: codes for high grade and high pressure issues for trans-national continental gas pipelines connecting remote production areas to consumption markets. ... Co2/HCO-3 environment”, Proceedings of “NACE CORROSION/97”, National Association of Corrosion
  21. Modelling Precipitation ofCarbides in Martensitic Steels Shingo…

    www.phase-trans.msm.cam.ac.uk/2004/shingo.pdf
    7 Jun 2010: at 180–250 C. The final hardness is about 500–700 HV. The most important characteristic.