Search
Search Funnelback University
- Refined by:
- Date: 2020
1 -
20 of
262
search results for `Download PDF file of paper` |u:www.phase-trans.msm.cam.ac.uk
Fully-matching results
-
Very Strong Low Temperature Bainite
www.phase-trans.msm.cam.ac.uk/2002/low.temperature.bainite.html14 Feb 2020: Such properties have never before been achieved with bainite. In this paper metallographic details are reported of the very fine bainitic microstructure associated with the incredibly low transformation temperature, where during ... the time scale of the -
Acceleration of Low-Temperature Bainite
www.phase-trans.msm.cam.ac.uk/2003/fast.bainite.html14 Feb 2020: Acceleration of Low-Temperature Bainite. C. Garcia Mateo, F. G. Caballero and H. ... In this work we report methods for accelerating the rate of reaction without compromising strength. -
Properties of Fine-Grained Steels Generated by Displacive…
www.phase-trans.msm.cam.ac.uk/2008/fine.html14 Feb 2020: strain. Some of the steels also can tolerate large fractions of brittle phases before fracture. ... Materials Science and Engineering A, Vol. 481-482, 2008, 36-39. Podcasts. A short audio interview of Harry Bhadeshia by Mathew Peet, on the content of the -
A Personal Commentary on "Transformation of Austenite at…
www.phase-trans.msm.cam.ac.uk/2010/Bain.html14 Feb 2020: study the progressive evolution of phases as a function of time and temperature. ... Download PDF file of paper, with permission from TMS International. -
Mechanical stabilisation of austenite
www.phase-trans.msm.cam.ac.uk/2006/stabilisation.html14 Feb 2020: The work has been used to explain why very large strains are required to mechanically stabilise certain stainless steels, and also to interpret the subunit mechanism of bainite growth. ... Materials Science and Technology 22 (2006) 641--644. Podcast. A -
Surface Relief due to Bainite
www.phase-trans.msm.cam.ac.uk/abstracts/swallow.html14 Feb 2020: High resolution observations of displacements caused by bainitic transformation. E. Swallow and H. ... Clear evidence has also been obtained of the plastic deformation induced in the adjacent austenite by the growth of bainite. -
Effect of 30 Tesla Magnetic Field on Transformations in a Novel…
www.phase-trans.msm.cam.ac.uk/2004/magnet.html14 Feb 2020: Effect of 30 Tesla Magnetic Field on Transformations in a Novel Bainitic Steel. ... Kelly, M. Murugananth and H. K. D. H. Bhadeshia. Abstract. The continuous cooling transformation characteristics of novel bainitic steels have been studied, both under -
Crystallographic Texture of Stress-Affected Bainite
www.phase-trans.msm.cam.ac.uk/2007/texture_bainite.html14 Feb 2020: or martensite under the influence of an applied stress or a system of stresses. ... selection. Proceedings of The Royal Society A, 463 (2007) 2309-2328. Podcast. A two-minute interview conducted by Mathew Peet, about the research documented in the paper. -
Mechanical Properties of Low-Temperature Bainite
www.phase-trans.msm.cam.ac.uk/2005/mechanical.html14 Feb 2020: Mechanical Properties of Low-Temperature Bainite. C. Garcia-Mateo, F. G. Caballero and H. ... Effect of 30 Tesla Magnetic Field on Transformations in a Novel Bainitic Steel". -
Hard Bainite
www.phase-trans.msm.cam.ac.uk/2003/hard.bainite.html14 Feb 2020: o. C. The time taken for nucleation at this temperature can be many days, but the transformation results in the growth of extremely thin platelets of bainite, so thin that the ... hardness of the resulting steel can be greater than 600 HV. -
Influence of Silicon on Cementite Precipitation in Steels
www.phase-trans.msm.cam.ac.uk/2008/silicon.html14 Feb 2020: K. D. H. Bhadeshia. Abstract. The mechanism by which relatively small concentrations of silicon influence the precipitation of cementite from carbon--supersaturated austenite and ferrite are investigated. ... Materials Science and Technology, Vol. 24, -
Low Temperature Bainite
www.phase-trans.msm.cam.ac.uk/2002/mateo.html14 Feb 2020: D. H. Bhadeshia. Abstract. It is demonstrated that bainite can be obtained by isothermal transformation at a temperature which is so low that the calculated diffusion distance of an iron atom, ... thin platelets of bainite, so thin that the hardness of -
Temperature Cycling and the Rate of the Bainite Transformation
www.phase-trans.msm.cam.ac.uk/2010/cyclic.html14 Feb 2020: Watson. Abstract. The possibility that the thermal cycling of supercooled austenite, within the bainite transformation range, accelerates the kinetics of decomposition is investigated both by analysing previous work and by conducting ... The cyclic -
Roughness of Bainite
www.phase-trans.msm.cam.ac.uk/2006/roughness.html14 Feb 2020: Download PDF file of paper.. ... Podcast. A short audio interview of Harry Bhadeshia by Mathew Peet on the content of the paper. -
Nucleation Theory for High-Carbon Bainite
www.phase-trans.msm.cam.ac.uk/2004/nucleation.html14 Feb 2020: In this paper we investigate whether the theory describing the nucleation of bainite is appropriate for this new class of materials. ... Download PDF file of paper.. -
High-Performance Bainitic Steels
www.phase-trans.msm.cam.ac.uk/2005/performance.html14 Feb 2020: Lee, H. K. D. H. Bhadeshia and H.-C. Lee. "Acceleration of Low-Temperature Bainite". ... Effect of 30 Tesla Magnetic Field on Transformations in a Novel Bainitic Steel". -
Neural Networks
www.phase-trans.msm.cam.ac.uk/abstracts/neural.review.html14 Feb 2020: Download PDF file of paper: ISIJ International,Vol. 39, 1999, 966-979.. ... Download PDF file of related paper: Statistical Analysis and Data Mining,Vol. -
Designing low carbon, low temperature bainite
www.phase-trans.msm.cam.ac.uk/2008/lowcarbon.html14 Feb 2020: The study also reveals the need for a better interpretation of the bainite start temperature to cover circumstances where the transformation times are unusually long. ... Materials Science and Technology, Vol. 24, 2008, 335-342. Podcasts. A short audio -
Silicon-Rich Bainitic Steel Welds
www.phase-trans.msm.cam.ac.uk/2003/Lord.Silicon.html14 Feb 2020: Svensson. Abstract. Ordinary bainite consists of a mixture of plates of ferrite and cementite particles. ... Download PDF file of paper. -
Kinetics of the Bainite Transformation
www.phase-trans.msm.cam.ac.uk/2004/bainite.kinetics.html14 Feb 2020: Predictions of the model are shown to compare well against published isothermal and continuous cooling transformation data. ... Download PDF file of paper..